 superalloy metals, superalloy powders, hastelloy, inconel, waspaloy, rene alloys, rene 41, rene 80, rene 95, rene 104, haynes alloys, incoloy, Ni-Cr-W superalloy, inconel superalloy, mp98t, tms alloys, cmsx, single crystal alloys, superalloy metals, FeNi-based superalloy, Ti-based-superalloy, Ni-based-superalloy, superalloy metals, Co based superalloy, single crystal superalloy, superalloy round, coated superalloy, melt-processed superalloys, wrought superalloy, superalloy ingots, high performance alloy, MIM,  superalloy metals, superalloy powders, hastelloy, inconel, waspaloy, rene alloys, rene 41, rene 80, rene 95, rene 104, haynes alloys, incoloy, Ni-Cr-W superalloy, inconel superalloy, mp98t, tms alloys, cmsx, single crystal alloys, superalloy metals, FeNi-based superalloy, Ti-based-superalloy, Ni-based-superalloy, superalloy metals, Co based superalloy, single crystal superalloy, superalloy round, coated superalloy, melt-processed superalloys, wrought superalloy, superalloy ingots, high performance alloy, MIM,  superalloy metals, superalloy powders, hastelloy, inconel, waspaloy, rene alloys, rene 41, rene 80, rene 95, rene 104, haynes alloys, incoloy, Ni-Cr-W superalloy, inconel superalloy, mp98t, tms alloys, cmsx, single crystal alloys, superalloy metals, FeNi-based superalloy, Ti-based-superalloy, Ni-based-superalloy, superalloy metals, Co based superalloy, single crystal superalloy, superalloy round, coated superalloy, melt-processed superalloys, wrought superalloy, superalloy ingots, high performance alloy, MIM, superalloy metals, superalloy powders, hastelloy, inconel, waspaloy, rene alloys, rene 41, rene 80, rene 95, rene 104, haynes alloys, incoloy, Ni-Cr-W superalloy, inconel superalloy, mp98t, tms alloys, cmsx, single crystal alloys, superalloy metals, FeNi-based superalloy, Ti-based-superalloy, Ni-based-superalloy, superalloy metals, Co based superalloy, single crystal superalloy, superalloy round, coated superalloy, melt-processed superalloys, wrought superalloy, superalloy ingots, high performance alloy, MIM,

  • Superalloy Metal and Powders Synonyms: 

superalloy metals, superalloy powders, hastelloy, inconel, waspaloy, rene alloys, rene 41, rene 80, rene 95, rene 104, haynes alloys, incoloy, Ni-Cr-W superalloy, inconel superalloy, mp98t, tms alloys, cmsx, single crystal alloys, superalloy metals, FeNi-based superalloy, Ti-based-superalloy, Ni-based-superalloy, superalloy metals, Co based superalloy, single crystal superalloy, superalloy round, coated superalloy, melt-processed superalloys, wrought superalloy, superalloy ingots, high performance alloy, MIM

  •  Superalloy Metal and Powders General Description: 

a) There are three types of superalloys- Fe-Ni based, Ni based and Co based. These are further divided into cast and wrought. A large number of alloys have been invented and many are patented and trademarked. Reade Advanced Materials (READE) makes a "best efforts" attempt to acknowledge all trademarks. Fe-Ni based are strengthened by intermetallic compound precipitation in a matrix. Ni based superalloys is the most important class. The Co based superalloys are invariably strengthened by a combination of carbides and solid-solution hardeners.

b) A superalloy, or high-performance alloy, is an alloy that exhibits excellent mechanical strength and creep resistance at high temperatures, good surface stability, and corrosion and oxidation resistance. Superalloys typically have a matrix with an austenitic face-centered cubic crystal structure. A superalloy's base alloying element is usually nickel, cobalt, or nickel-iron. Superalloy development has relied heavily on both chemical and process innovations and has been driven primarily by the aerospace and power industries. Typical applications are in the aerospace, industrial gas turbine and marine turbine industry, e.g. for turbine blades for hot sections of jet engines.

c) Examples of superalloys are Hastelloy, Inconel, Waspaloy, Rene alloys (e.g. Rene 41, Rene 80, Rene 95, Rene 104), Haynes alloys, Incoloy, MP98T, TMS alloys, and CMSX single crystal alloys. Source: Wikipedia

  • Superalloy Metal and Powders Typical Chemical Purities Available:  

Available from READE to customer specification

  • Superalloy Metal and Powders Typical Granulations Available:

Targets, tablets, pieces, and various standard powder granulations.

  • Superalloy Metal and Powders Typical Applications:

a) Used in cast, rolled, extruded, forged and powder-processed forms. Numerous aerospace applications (sheet, bar, plate, tubing airfoils, turbine disks, seals, blade retainers, turbine vanes, turbine blade dampers) have continued to be very successful.

b) Used in cryogenic equipment, orthopedic and dental prostheses.

c) Metal injection moulding (MIM) of near net shape parts.

  • Superalloy Metal and Powders Packaging Options:

Jars and drums

  • Superalloy Metal and Powders TSCA (SARA Title III) Status:

Listed. For further information please call the E.P.A. at +1.202-554-1404

 

 

 

Translate

English French German Italian Portuguese Spanish

Text Resize

Request a quote from READE Advanced Materials
READE Science and Technology Bookstore

Join Us On...

Join us on The Nanomaterials Society

Follow Us On...

Follow our updates on Twitter